Process of sand casting aluminum.
2000 degrees farenheight
1120 degrees farenheight
650 degrees farenheight
2500 degrees farenheight
0 degrees celcius
A hem
Draft
Pattern relief
All of the above
None of the above
Lost wax casting
Green sand casting
Investment casting
All of the above
None of the above
Riddle
Sieve
Screed
All of the above
None of the above
It could burn the concrete
It could explode and burn those around it
It could harden and ruin the floor
All of the above
None of the above
Strike off bar
gate cutter
Bench rammer
Sprue cutter
Riser
Gate
Sprue
Vent
Cope and drag
Top and bottom
Bow and limb
All of the above
None of the above
Riser
Gate
Sprue
Flask
Pattern